I am trying to electroplate a silver on a glass slide. I am using
Ammoniacal SIlver Solution (0.72mol/L of NH3 (150ml) + 0.93gm of
Silver nitrate crystals). THe electroplating is carried out at 0.1 A
and 1.74 V. But the silver which is plated on my slide is not uniform.
It appears to me like a mesh. Could someone tell me  proper contents
for the silver plating bath with their accurate proportions?

--