Apiezon Wax W will soften at 80C and melt at 100C, not sure of its PCR
compatible properties.



-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Yue Mun Pun, Jeffrey
Sent: Thursday, 7 June 2007 3:24 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] High temperature wax with melting point ~100'C and
PCRcompatible

Hi,
I am looking for a wax which has melting point of about 100'C or
slightly higher and which is compatible with PCR.