Hi
    You can see for Anodic Bond too.
Regards

NH
>
> -----Original Message-----
> From: mems-talk-bounces@memsnet.org
> [mailto:mems-talk-bounces@memsnet.org] On Behalf Of P.E.M. Kuijpers
> Sent: 20 August 2007 13:07
> To: mems-talk@memsnet.org
> Subject: [mems-talk] Glass to glass bonding
>
> Hi all,
>
> Is there a way to bond two glass wafers (Eagle glass ) directley to each
> other without any intermediate layer??