durusmail: mems-talk: black wax for koh etch
black wax for koh etch
2007-11-05
2007-11-07
2007-11-07
black wax for koh etch
Chin-Jen Chiang
2007-11-05
Hi guys,

  For some reasons I can't use nitride or oxide layer as etch mask for KOH
etching in my process and plan to use black wax as etch mask. Do you know where
I can get the black wax. Dose the black wax need to be special one or the
regular black wax used to wax car is fine. I will appreciate your advice.
Thanks.

  Regards
  Lawrence