Hello, I am seeking an organization that would be willing to do deep boron diffusions for a commercial firm. These diffusions are 15um deep with a doping level of greater than 3E19 cm-3. The company would like to process 250 wafers per year. Thank you Andrew Oliver Electromechanical Engineering Department Sandia National Laboratories Albuquerque, NM 87185-0329 Phone: (505) 845-7931 FAX: (505) 844-9554 adolive@sandia.gov