Happy New Year to all I used UV-tape as barrier during DRIE process. But I could not remove it easily even though I did piranha cleaning 10min and soak in acetone over 5hr.(did acetone first^^) I assume adhesion properties of UV-tape get changed during DRIE process so, it is difficult to remove UV tape completely. So I can remove UV-tape completely? Best regards, Ero