wouldn't just oxide work for you? if the phosphoric acid is pre-conditioned, oxide is an excellent etch stopper. _iv On Jan 8, 2008 7:48 AM, Sandip Agarwalwrote: > I want to pattern silicon nitride by etching with hot phosphoric acid. > What are the photoresists that would withstand these etching conditions?