Hi All,

  Does anyone know of any chemical supplier/vendor selling ready-made phase-
change plating solution? e.g. GeTe, Sb2Te3, Ge2Sb2Te5, etc.

  I could not find any in the internet, so I currently mix the elemental powder
with some acids and then used the mixture solution for phase-change material
electrodeposition. But it's  a tedious work, so It'll help much if there's any
commercially available phase-change material plating solution.