What do you want to attach together? I used crazy glue from walmart, it works fine for tubing!! Have fun, -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Hong Chen Sent: Wednesday, May 28, 2008 11:37 AM To: mems-talk@memsnet.org Subject: [mems-talk] PDMS glue recommandation Hi, is there anyone can recommend a PDMS glue? I found epoxy-based and ethylene- vinyl- acetate-based is not useful. Well, you can use PDMS as the glue but the problem is it trends to spread and occupy every spaces it can reach including your micro channels. Hong