durusmail: mems-talk: Wet Etch of Ta2O5 Thin Film
Wet Etch of Ta2O5 Thin Film
2008-06-12
Wet Etch of Ta2O5 Thin Film
Gord Wang
2008-06-12
We are in the process of developing Ta2O5   thin film deposition process
using RF sputtering. Does anybody know the chemicals/recipes used to wet
etch Ta2O5 thin films?

Your help is highly appreciated!

Thanks,

Gord Wang
Thin Film Process Engineer
Nanowave