durusmail: mems-talk: Ni plating on Au film
Ni plating on Au film
2008-07-16
2008-07-18
2008-07-20
Ni plating on Au film
汪飞
2008-07-18
Sorry but what is Ni strike?

2008/7/17, Qi Luo :
> In our structure, we electroplate Ni on Au substrate. Our process has
> Alkaline clean, another step of activation, Ni strike, then Ni plating. For
> our application, the adhesion of the plated Ni to Au film is very important.
> Can we replace the Ni strike with Au strike, or insert a Au strike before Ni
> strike to improve adhesion? Your help would be greatly appreciated.
> With kind regards,
> Qi Luo

Best regards,
Yours sincerely
Fei Wang
______________
State Key Lab of Transducer Technology,
Shanghai Institute of Microsystem and Information Technology,
Chinese Academy of Sciences
865 Changning Road, Shanghai 200050, China
Email:wangfeiustc@gmail.com
Tel:0086-21-62511070 ext.5468
reply