How to improve ohmic contact, gold - chrome coating on silicon?
Suraj Patil
2008-07-28
Hi Moshe,

Try annealing the sample at 150 C-250 C for 10-15 minutes, presence of
N2 would help.

Suraj

On Sun, Jul 27, 2008 at 2:59 PM, Moshe  wrote:
> How can I improve ohmic contact where the coating is gold - chrome on silicon
?
>