Hi : you can prepare the PMMA solution in acetone firstly, and deposited on glass slide by spin coater Depends the thickness of the PMMA film that you want, you can change the concentration of PMMA solution Also , you can buy the commercial PMMA solution Dazhong Wu wrote: > Hi there, > > Does anyone have experience of depositing PMMA on glass slide to prepare PMMA films? > I got the following information in a reference: > " depositing droplets of 10g of PMMA in 15g of acetone on glass slide and letting acetone evaporate over a few days" > > But what exact deposit method should I use? what instrument should I use? I have no this kind of knowledge before, So I appreciate someone can tell me the details. > > Sincerely, > Dazhong Jian Shi Laboratoire de Photonique et de Nanostructures UPR20/CNRS Route de Nozay 91460 Marcoussis - France tel: 01 69 63 60 09 fax: 01 69 63 60 06 http:// www.lpn.cnrs.fr