This will evaporate any moisture presenting on surface of a wafer and
thus promotes adhesion of photoresist.

Evelyn B wrote:
> I have seen dehydration bakes used as part of solvent cleaning of glass and
> sapphire substrates. What is the purpose/advantage of this bake?
>