Pyrex is a borosilicate glass. You can bond the Pyrex directly to the silicon wafer without the need to deposit additional borosilicate glass. In fact borosilicate isn't absolutely necessary for anodic bond. Any mobile ion containing glass should work. Roger Shile -----Original Message----- Hi everyone, I am going to evaporate or sputter a kind of Borosilicate glass (or similar) on pyrex to anodically bond pyrex to si wafer. Does anyone knows where I can buy some sample of the glass for evaporation or sputtering? Any help will be highly appreciated. Thanks, Reza Rashidi