Its Trion Phantom
Thanks

On Sun, Mar 8, 2009 at 5:49 PM, Jie Zou  wrote:

> What is your RIE machine? I worked two months to get a reliable recipe for
> the Unaxis Shuttlelock RIE/ICP.
>