Hi, I used to ebeam to deposit Al on the glass substrate. I found some black
stuffs distributed on the entire Al surface after deposition. Following dry
etching transfer these to the glass substrate and make the surface very rough. I
do not what are these black stuffs and how to get ride of them. Anyone has the
similar experiences and solution.

Thanks!

shifeng