bonding su-8 layer with pdms?
2009-06-22
2009-06-23
2009-06-23
bonding su-8 layer with pdms?
김태진
2009-06-22
Hi all!

Has anyone tried bonding a Su-8 layered substrate with PDMS?

I made a attempts by treating a su-8 film coated wafer with pdms using oxygen
plasma (30W for 1 min), but the devices seemed not bond at all.

Does anyone have suggestions?

Thanks!
Best regards,

TJ
reply