Hi everybody, I am pretty new to soft lithography using PDMS. Can anyone kindly tell me the exact meaning of complete curing of PDMS? or rather how can I be sure that my PDMS has completely cured? I have seen papers reporting that under certain conditions there was uncured PDMS left behind particularly at the edges of a master mould while peeling off the PDMS layer. Also I suppose that for PDMS deposition of different heights the curing duration also is different. Can anyone kindly suggest me some optimum range of temp , time and PDMS thickness for complete curing of PDMS? Looking forward for your help, Thanks in advance. Debashis Maji, JRF, School of Medical Science & Technology, IIT Kharagpur, India - 721302