Ruiz, Marcos Daniel (SENCOE)
2009-08-27
A quartz beaker will not work for use in any HF mixture.

Dan

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of David Casale
Sent: Thursday, August 27, 2009 8:02 AM
To: mems-talk@memsnet.org
Subject: Re: [mems-talk] Dipper basket/vessel 4" in diameter

Just any quartz beaker should work, right?