Hi Lin,

Try to search "electroless plating" both in English and in Chinese. I
think you can get some information.

Pt could be used as a catalytic layer for nickel plating. The
catalytic layer doesn't have to be connected. You just deposit it
where to plate. Maybe you can try with a lift-off technique.

Best regards,
Fei

2009/10/14, lin yu :
> Rick,
>
> If I deposit a thin layer of metal on high doped Si (but the metals
> are not connected together),
> can I use Si as the conductive layer for electroplating?  Will this work?
>
> Thanks,
> Lin

--
Best regards,
Yours sincerely
Fei Wang
______________
Postdoctoral researcher, Dr
MIC - Department of Micro and Nanotechnology
Technical University of Denmark (DTU)
Building 344, 1st floor, Room no. 130
DK-2800, Kgs. Lyngby
Denmark
Tel:  +45 4525 6311
Fax:  +45 4588 7762
Email: fei.wang@nanotech.dtu.dk
       http://www.nanotech.dtu.dk
reply