Mohammed, How thick PDMS? Shay -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Mohammed Asfer Sent: Wednesday, October 28, 2009 8:36 AM To: mems-talk@memsnet.org Subject: [mems-talk] Drilling holes in PDMS hello all I want to make holes of 1.6 mm diameter in PDMS layer. Is there any technology available for this? Regards Asfer