Hey Guys, I am also looking for Silicon Nanowire generation for my project. I am looking for a good recipe to achieve that. Any help will be appreciated greatly. Thanks Anirban On Thu, Nov 5, 2009 at 4:37 AM, rahul goswami goswamiwrote: > Hi all, > > I had formed porous membrane using HF :Propane (1:1) and done > electrochemical etching for duration of 10 minutes by passing 10mA/cm2 > current density. > > However, the porosity observed in SEM pic is not good. Any suggestions on > improving the electrochemical etching? > > regards > rahul > ANIRBAN Electrical Engineering Louisiana State University Baton Rouge 70802,USA