Hi Bob.

Doesn't SU-8 require an additional spun-on layer of SU-8 in order to bond
after developing? I was looking at SU-8 from the beginning but couldn't
find a decent way of bonding the structured/developed SU-8 to the second
glass wafer? I'm looking at a glass - SU-8 - glass structure.

Thanks!

/Mikael

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of Bob Henderson
Sent: Friday, December 04, 2009 3:20 PM
To: 'General MEMS discussion'
Subject: Re: [mems-talk] thick structurable films

Try SU-8