durusmail: mems-talk: Ag wet etch
Ag wet etch
2010-09-16
Ag wet etch
Mingke Xiong
2010-09-16
Hi, All,

Does anyone know a good silver wet etch recipe? Better has good selectivity to
Cu.

Thank you.

Regards,

Mingke Xiong
AEM, Inc.
6610 Cobra Way
San Diego, CA 92122, USA
www.aem-usa.com
858-481-0210 (1660)
reply