Selective Poly etch for P+
Morrison, Richard H., Jr.
2010-09-21
What recipe did you use?
Rick
-----Original Message-----
From: mems-talk-bounces+rmorrison=draper.com@memsnet.org
[mailto:mems-talk-bounces+rmorrison=draper.com@memsnet.org] On Behalf Of
morad massalha
Sent: Tuesday, September 21, 2010 12:03 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Selective Poly etch for P+
I have read about this mix that etch P+ 1E18 and stop on P- (1E14). I
tried this
while etching a silicon wafer with EPI. I took silicon and I put it in
the mix for 5
min. The result was that wafer etched on both sides with same thickness.
Maybe
from P+ etched more about 30%, but I did not get any selectivity between
P- and
P+. Can somebody explain this please.