Watch out for the zinc - it tends to vaporize easily and contaminate anything it comes in contact with >Hello, > > I would like to post a message up for discussion. I need to find a >liquid metal (alloy) with a low melting temperature. Or a conducting >liquid with a very low vapor pressure so that it does not easily >evaporate. I already know of the Indium, Gallium, and Tin eutectic (and >also the one with zinc). But if anyone knows of a better choice of a >conducting fluid, all tips with be greatly appreciated. > >Thanks > >Trung D. Truong > >