Hello Vijay, If it is a polymer then oxygen plasma etching is probably a good choice. You will need a resist somewhat thicker than the BCB assuming you would prefer not to use a metal masking layer. -Michael >>> Vijay Rajaraman11/22/2010 6:12 PM >>> Hello, Has anyone successfully etched (selective or blanket) 10 microns of cured BCB (cyclotene) or UV glue, landing on either Si or Al, without residues ? In case of selective etching, the preferred masking material is photoresist. Is there any good reference material on etching such thicker polymer layers? Do let me know. Many thanks, Vijay