2010-12-01
If you do a google search for "process wafer carrier" it should give you
the information you seek

Dan Ruiz

________________________________

From: mems-talk-bounces on behalf of Albert Henning
Sent: Wed 11/24/10 12:56 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] source for carriers for die cleaning?


We are looking for a commercial source for die carriers appropriate for
RCA-type cleaning.

The die have various sizes, up to several cm square.  We'd like them to
stand upright in the cleaning baths, as a wafer would in a wafer
carrier.

Thanks in advance.