Hi,
I was electrodepositing Ni at a nanometer scale. It depends on
solution used, Voltage applied,  substrate etc.

But if you find the right parameters you fey very uniform thin layers

La data de 26.04.2011, 22:55, Xiaohui Lin  a
scris:

> Does anyone have experience electroplating Ni with thickness less than
> 1um? How is the uniformity and surface roughness?