Hello,

Does anyone have experience of using Ma-N400 series negative resist for lift-off
process? Without ultrasonic bath, is it possible to get a clean lift-off result
for Ti/Au (10nm/100nm)?  I am using Rem660 remover at 80C, but I cannot see
metal removed in 10mins. Should it take longer time?