Dear All, Hope you all are doing great. I was wondering if any one of you has worked for SU 8 release? I am currently using LOR 5A but then i have been told that LOR B is better since its dissolution rate is high. Can somebody suggest, out of omnicoat and LOR which is better for release of single SU 8 layer of thickness 50-100um (not multistructural layer, hence the released SU 8 will be a bit brittle). Thanks a lot in advance. ANy comment is welcome even if it involved the use of different release method! Kind Regards, Sumit