thin aluminum foil
Sam Miller
2012-03-21
You can evaporate salt.

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Lukasz Urbanski
Sent: Wednesday, March 21, 2012 2:03 PM
To: General MEMS discussion
Subject: [mems-talk] thin aluminum foil

Hi Guys,
I'm trying to fabricate thin (100-300 nm) aluminum foil. I have seen
some evaporated on a glass substrate (regular micro slide), which can
be lifted off by simply floating them in water. I am guessing, that
there is some coating  (parting off agent) applied on the glass prior
to evaporating aluminum. I wonder what parting off agent should I use
and how to apply it. Do you have any suggestions?
Thanks,
-Lukasz
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply