Dear all,Could anyone advise the shear strength of silicon? Any orentation would be ok.I've been searching for the data in vain.Thanks in advance for any help.All the best,WANG, Yingnan _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk