Hi Yingtao, Maybe you can use O2 Plasma, but it is going to damage the thin oxide film on the top of the chrome. which is the thickness of the crosslinked SU8? Best regards, Karim On Tue, Jul 17, 2012 at 11:16 AM, Yingtao Tianwrote: > Hi All, > > I have a chrome/glass mask seriously contaminated by crosslinked SU8, anyone has an idea how to rescue the mask? > > Thanks, > Yingtao > > > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk