Daniel: At this time we have only run fluorocarbon films using C4F8 in our reactor. The water contact angle was 105 degrees and I don't know what the hysteresis was. We are looking to partner with groups to complete the SiOx + C-F work looking toward building a larger production type system. Currently we can run up to 8" x 8" samples. Can you discuss what your application is? Substrate being treated? Bob Henderson -----Original Message----- From: mems-talk-bounces+bob.henderson=etchedintimeinc.com@memsnet.org [mailto:mems-talk-bounces+bob.henderson=etchedintimeinc.com@memsnet.org] On Behalf Of Daniel Figura Sent: Monday, June 10, 2013 3:10 AM To: 'General MEMS discussion' Subject: Re: [mems-talk] Super hydrophobic films in a new PECVD reactor Hello Bob, what is the hysteresis of water contact angle on the surface? What size of samples can you make (6"x6")? Thank you. With best regards, Daniel Daniel Figura smartfabgroupT Company process consulting . data processing . fab software Phone: +421 944 45 26 86 E-mail: daniel.figura@smartfabgroup.com, Web: www.smartfabgroup.com Disclaimer notice: The information contained in this message and any attachments is intended only for the personal and confidential use of the designated recipient(s) named above. If you are not the intended recipient of this message you are hereby notified that any review, disseminitation, distribution or copying of this message is strictly prohibited. If you have received this message by error, please notify the sender immediately. -----Original Message----- From: mems-talk-bounces+daniel.figura=smartfabgroup.com@memsnet.org [mailto:mems-talk-bounces+daniel.figura=smartfabgroup.com@memsnet.org] On Behalf Of Bob Henderson Sent: Friday, June 07, 2013 00:53 To: mems-talk@memsnet.org Subject: [mems-talk] Super hydrophobic films in a new PECVD reactor Is there anyone within the MEMS community that is looking for a film composed of a silicon oxide and fluorocarbon sandwich which produces a hydrophobicity with a contact angle >150 degrees. In particular would this type film be useful for micro fluidic channels as a barrier or to increase flow rates in small openings? Bob Henderson _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk