durusmail: mems-talk: Electroplating Dielectric Material
Electroplating Dielectric Material
2014-09-15
Electroplating Dielectric Material
Robert Bock
2014-09-16
I'd recommend looking into a PVD process to deposit a dielectric, not
electroplating.

Robert


-----Original Message-----
From: mems-talk-bounces+mastering=dvdfactoryinc.com@memsnet.org
[mailto:mems-talk-bounces+mastering=dvdfactoryinc.com@memsnet.org] On Behalf
Of Ricky Anthony
Sent: Sunday, September 14, 2014 9:55 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Electroplating Dielectric Material

Hi,

I was wondering if there is any dielectric (or poor semiconductor) which can
be electroplated on conductive surface like Nickel. Could you give brief
process for it?

Thanks,

Ricky Anthony

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply