Hi Ali,

Take a look at http://www.smalltechsupplies.com/91-services
It's 4"and 6", affordable pricing.
We sell in 10 packs but maybe you can share with other students.


Best regards,

Willem Poterman
SmallTechSupplies

Webshop www.smalltechsupplies.com
Tel. +31 6 1203 5376

-----Oorspronkelijk bericht-----
Van: mems-talk-bounces+info=smalltechsupplies.com@memsnet.org
[mailto:mems-talk-bounces+info=smalltechsupplies.com@memsnet.org] Namens Ali
Alsaqqa
Verzonden: maandag 29 juni 2015 07:55
Aan: mems-talk@memsnet.org
Onderwerp: [mems-talk] low-quantities Silicon wafer supplier

Hello all,

I am looking to buy a silicon wafer (1" or 2" diameter, not necessarily
prime quality). Whenever I look online it seems companies only sell in packs
of 24 or 25 wafers, which is very expensive for a student like me.
Does anyone know of a supplier who sell individual wafers at an affordable
price?

-Ali
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply