suitable etchant for titanium thin layer on silicon substrate
Shay
2016-06-02
Hi
You can try BOE. (HF 10:1 or 6:1)

Shay

> On May 29, 2016, at 16:20, KarthiKeyan K  wrote:
>
> Dear Friends,
>
> Kindly suggest suitable etchant for titanium thin layer on silicon substrate.
(PPR mask pattern over the titanium thin layer)
>
> Looking forward to you reply.
>
> --
>
> Thanks & Best Regards,
> KarthiKeyan K
>
> ​ Please consider the environment before printing this email  -
Save Trees, Save our Planet Earth !!!
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply