Hi Caleb,

we recently deposited copper oxide by reactive sputtering. An important
question is if copper(I)- or copper(II)-oxide is needed.

Regards,
André

-----Ursprüngliche Nachricht-----
Von: mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org
[mailto:mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org] Im
Auftrag von Guo
Gesendet: Montag, 27. Juni 2016 21:21
An: General MEMS Discussion
Betreff: [mems-talk] Oxide growth

Hi all,

We are looking for someone to help us to do thin film oxide growth: copper
oxide and cobalt oxide. If you or you know someone who might be able to do
that, please let us know ASAP.

Thank you in advance.

Best regards,Caleb
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply