Hello Kevin, I am not certain as to how this vendor achieves the holes in their materials, but they are a well established vendor for drilled sapphire, they may be able to help. Insaco Inc. 1365 Canary Road PO Box 9006 Quakertown, PA 18951-9006 Contact: Scott D. Mittle 215-536-3500 phone 215-536-7750 fax sdm@insaco.com = e-mail Best regards, Constant Reyerse Sales Engineer, Midwest Karl Suss America, Inc. 228 Suss Drive Waterbury Center, VT 05677 Phone: 802-244-5181 ext. 403 Phone: 317-246-7741 Indianapolis Office Fax: 802-244-5103 >>> "Kevin M. Walsh"09/09/99 11:18PM >>> Does anyone know of a vendor that manufactures an Ultrasonic Drilling Machine appropriate for drilling relatively-small holes (1 mm in diameter) into glass wafers. Thanks, Dr. Kevin M. Walsh Associate Professor of Electrical Engineering Director of the Lutz Microtechnology Cleanroom University of Louisville Lutz Hall, Room 436 Brook St and Warnock Ave Louisville, KY 40292 (502) 852-0826 office (502) 852-1577 fax email: walsh@louisville.edu or walsh@ieee.org WWW: http://mitghmr.spd.louisville.edu