durusmail: mems-talk: summary of stress removal from glass
summary of stress removal from glass
1999-11-11
summary of stress removal from glass
Debjani Pal
1999-11-11
Hi,

I want to thank everyone who has responded to
my mail about removing stress from glass.
A summary of all the suggestions I got is
given below.


Debjani Pal

Research Scholar (Semiconductor Group)
Department of Physics                 Ph: (080)309-2316
Indian Institute of Science           Fax:(080)334-1683
Bangalore - 560012


reply