Send reply to mems@isi.edu Hi there, I am looking for information about reactive-sputtering of Iridium in an oxygen atmosphere. Espacially information about running that process would be helpfull. Since we are also searching for a second-hand sputtering unit, related offers are welcome too. Thank's for reading the request, have a merry christmas and a happy 1996 Otto Wassmus