If you get any information I would be interested in getting a copy of it. We are currently using a frit paste from Nippon Electric Glass (NEG) for sealing applications. Product code LS-1301. Contact: Isao Suzuki [isuzuki@neg.co.jp] or Wes Jelinsky (wjelinski@negamerica.com). -Kevin