Winston: We have been using the SCS Spin coater and it works great. I strongly recommend the SCS spin coater and the price is great. They also have a great leasing plan (~$500 for 3 months), you may lease it to check it out. Jayant ***************************************** Jayant Neogi Vice President & Chief Technical Officer Ph# 503-640-0586 Fax 503-640-8117 http://www.norsam.com ***************************************** Winston Chan wrote: > > Our photoresist spinner died last week and we are looking for a new one. > I found several manufacturers of small benchtop spinners - Headway, > Laurell, Cost Effective Equipment (part of Brewer Science) and SCS > (Specialty Coating System). Does anyone have experience, good or bad, > with these spinners? Are there others that I should be looking into? > > Winston > > -- > Winston Chan | phone: (319) 353-2398 > Dept. of Electrical Engineering | fax: (319) 353-1115 > University of Iowa | email: wkchan@icaen.uiowa.edu > Iowa City, IA 52242 > --