Hi,

My name is Bala and i work in the Mirowave and Wireless Group at USF. I'll
appreciate if anyone can give me the reciepe for etching <100> silicon using
CF4. The trench i am etching is more than 100um deep.

Thanks in advance for the help

 --Bala