Hello Andreas, My name is Mario Robles and I work for Tanaka Systems Inc. We represent Asahi Diamond dicing blades and grinding wheels in the U.S. Asahi can manufacture both metal and electroplated blades to cut the material you have questions on. Our website is www.dicingblades.com and it basically has pictures of the various products we sell. You can contact Mr. Go at Asahi to find out who would be your contact regarding Ashai blades in your area. A standard blade used to cut your material would be as follows: SD400L50MST-16S 56.0D 0.250T 40H Fed Speed 1"~3"/sec RPM 24~30K Mario Robles Technical Sales Manager -----Original Message----- From: Andreas Albrecht [SMTP:tzm.albrecht@t-online.de] Sent: Friday, June 09, 2000 1:01 AM To: MEMS@ISI.EDU Subject: PCB dicing blades experiences Dear MEMS Folks, could anyone give me an advice who supplies dicing blades (2 or 4") for cutting blended, through hole plated PCBs (1-3 mm thickness). Who has made good experiences (tool life, duration) with which blades? Are there any good application informations on the web? -- Regards Andreas Albrecht Transferzentrum Mikroelektronik e.V. In den Weiden 7 D-99099 Erfurt Tel. +49-(0)361-44 20 660 Fax +49-(0)361-44 20 666