durusmail: mems-talk: Metal electrodes onto thick SU-8 resist
Metal electrodes onto thick SU-8 resist
Metal electrodes onto thick SU-8 resist
Dekker, R. (Ronald JDSU)
2000-10-23
Hi there MEMS people,

Is there anybody who has some experience on evaporating or sputtering
metals onto SU-8 resist? Is there any data on adhesion of metals on this
resist
type? Which metals show good adhesion and which adhere badly?

Any info would be greatly appreciated,

Cheers,
Ronald Dekker   <<< Ronald.R.Dekker@AkzoNobel.com
  >>>