Our lab needs lots of the following two types of PZT & Silicon specimens
for testing.

* Two PZT ceramic beams (4mm*1mm*0.5mm) adhered onto a silicon beam
(4mm*0.8mm*0.5mm). The width of the silicon beam is smaller than the one
of the PZT beams. A mask between the PZT/Silicon interface will form a 1mm
long, through the width, delaminaiton.

* Two silicon beams (4mm*0.8mm*0.5mm) adhered onto a PZT beam
(4mm*0.8mm*0.5mm).  A mask between the Silicon/PZT interface will form a
1mm long, through the width, delaminaiton.

If you know some companies who can manufacture the above specimens
for our lab, please tell me. Your help will be much appreciated.