Hi,
I did not have problem use Au as protective etal from TMAH. But do not
know exact reaction.
mori

On Thu, 8 Feb 2001 xuwh@ust.hk wrote:

>
> Hi, this is xu wehua,from Hong Kong Science and
> Technology.
>
> WOuld you please tell me if TMAH and Au have a
> reaction?? If have a reaction,what is the
> reaction rate??
>
> Does any one know if gold is etched by TMAH ??
>
> Regards,
>
> Xu Weihua
>
>

============================================
Kiyotaka Mori (Graduate Research Assistant)